Anodising classifications
- Type I and IB
- Chromic acid anodising. Thinner coating films, preferred where fatigue resistance matters, such as connection and structural elements on aircraft.
- Type IC
- Non chromic acid substitute for Types I and IB, where a non chromate alternative is required.
- Type II
- The conventional sulfuric acid bath coating, and the most versatile for colour.
- Type IIB
- Non chromate alternative to Type I and IB coatings, aligned with environmental protection standards.
- Type III
- Hard anodising. A thicker coating aimed at wear resistance, at the cost of some fatigue life.
Types I, IB and II are all used where a component needs corrosion resistance to a certain extent. Type III is primarily about wear, which makes it the choice for gears, valves and other parts subject to sliding action, and the wrong choice where fatigue life is the governing requirement.
Compared to uncoated aluminium, every type improves the adhesion of paint and other bonding agents. Some parts need further treatment after anodising, such as colouring, sealing, or dry film lubricants. If colouring is needed the part falls under Type II; uncoloured components are classified as Type I.
Anodising thickness and dimensional change
Anodising changes the size of the part, and it is the first thing to design around. Engineers usually account for this by specifying post treatment dimensions on the drawing. In rapid prototyping, where solid models are used instead of detailed drawings, that adjustment has to be made in the model instead.
Anodising expands the surface area of the treated part. External dimensions such as the outer diameter of a cylinder increase, while internal features such as holes decrease, because the oxide layer grows both inward and outward from the original surface.
The expansion is proportional to the thickness of the anodic layer, and can increase the overall dimension by up to 50% of that layer thickness. Layer thickness itself varies with the alloy and the controls applied during processing, so where precision is paramount that variability has to be allowed for.
With thicker Type III coatings, post treatment machining such as grinding is sometimes needed to reach the final size. That is an additional step, and it adds both time and cost, so it is worth deciding early whether the part needs it.
Anodising is less effective on sharp corners, and more so for thicker Type III coatings. Designers should consider the radius of edges and internal angles and avoid sharp corners where the coating will be weak. Corner radii for different Type III thicknesses are guided by standards such as Mil-A-8625.
Hard anodising for wear resistance
Hard anodising creates an oxide layer that increases surface stiffness, which is why it is chosen for parts that need wear resistance. Its adhesion is the distinguishing feature: roughly 50% of the oxide layer penetrates into the aluminium alloy while the remaining 50% sits on the surface. Applications include baseball bats, bicycle frames and flashlights.
The process typically produces a layer 30 to 50 micrometres thick with a hardness around 500HV, with strong corrosion and wear resistance. The layer is non toxic and safe for human contact, which puts it in kitchen appliances, medical device packaging, air and oil cylinders and printing rollers. It holds up under high pressure and temperature.
The dimensional change is larger than with thinner types, so allowance calculations matter more. This is a design stage decision, not something to discover at inspection.
Hard anodised aluminium alloy is increasingly replacing stainless steel in specific components, offering a lighter but durable alternative. The wider field includes thermochemical hard oxidation, PVD, CVD, diamond film coating and multilayer composite coatings, which offer more toughness and wear resistance than processes such as conductive oxidation, whose layer is far thinner at 0.01 to 0.13 micron.
Colour anodising and dyeing
Anodic oxide films can be coloured, and that is more than a cosmetic point. The obvious benefit is appearance, which matters on consumer facing products where it influences buying decisions. In optical systems, coloured films reduce stray light, which improves the accuracy of instruments. And colour aids recognition of components during assembly, which in a complex build reduces errors.
The main constraint is fading. Anodic oxide films tend to fade under UV light or high temperature, and organic dyes fade more than inorganic ones. Since most vibrant colours are only achievable with organic dyes, there is a trade between the colour you want and how long it lasts.
Which type you specify decides what colour you can have. Type I, with its thinner coating, struggles to reach deep black; even with black dye the result often reads grey. Type III, with its thicker coating, tends toward dark grey or black on certain alloys, which restricts the range, though thinner Type III coatings can sometimes take more than one colour.
Type II is generally the most versatile and effective for colour, with better dye absorption and retention across a broader range.
Conductivity and composite coatings
Despite the conductivity of the base metal, the anodic oxide layer is a highly effective insulator. That is a benefit for electrical safety, but a problem where grounding is essential, such as on electronic components or a metal chassis.
The answer is a transparent chemical transmission layer applied to targeted areas of the component. It keeps the insulating properties of the anodic layer overall while allowing conductivity in the specific zones that need grounding. It has to be applied precisely, so that it only covers the areas where transmission is required.
Anodised parts also take secondary treatment. Paint over the anodic coating reaches colours that conventional dyeing cannot, and can increase corrosion resistance at the same time.
Teflon immersion is the other common one, and it is particularly effective on Type III hard coatings. It significantly reduces the friction coefficient of the surface, which matters on moving parts, in mould cavities, and anywhere components slide against each other.